Transactions of the American Society of Civil Engineers, Vol. LXX, Dec. 1910 - Final Report of Special Committee on Rail Sections, Paper No. 1177 by Various
page 14 of 17 (82%)
page 14 of 17 (82%)
|
[Sidenote: Tests.] "13. (A) Two pieces shall be tested from each heat of steel. If either of these test pieces breaks, a third piece shall be tested. If two of the test pieces break without showing physical defect, all rails of the heat will be rejected absolutely. If two of the test pieces do not break, all rails of the heat will be accepted as No. 1 or No. 2 classification (according as the deflection is less or more, respectively, than the prescribed limit[A]). "(B) If, however, any test piece broken under test A shows physical defect, the top rail from each ingot of that heat shall be rejected. "(C) Additional tests shall then be made of test pieces selected by the Inspector from the top end of any second rails of the same heat. If two out of three of these second test pieces break, the remainder of the rails of the heat will also be rejected. If two out of three of these second test pieces do not break, the remainder of the rails of the heat will be accepted, provided they conform to the other requirements of these specifications, as No. 1 or No. 2 classification (according as the deflection is less or more, respectively, than the prescribed limit[F]). "(D) If any test piece, test A, does not break, but when nicked and tested to destruction shows interior defect, the top rails from each ingot of that heat shall be rejected. [Sidenote: Drop testing machine.] |
|